基本尺寸 | 基本额定载荷 | 额定转速 | 型号 | ||||
---|---|---|---|---|---|---|---|
dynamic | static | Reference speed | Limiting speed | Model | |||
d[mm] | D[mm] | B[mm] | C[kN] | C0[kN] | [r/min] | [r/min] | |
1120 | 1360 | 106 | 3350000 | 8500000 | SL1818/1120-E-TB | ||
1000 | 1220 | 100 | 2900000 | 7100000 | SL1818/1000-E-TB | ||
950 | 1150 | 90 | 2550000 | 6300000 | SL1818/950-E-TB | ||
900 | 1090 | 85 | 2320000 | 5700000 | SL1818/900-E-TB | ||
850 | 1030 | 82 | 2050000 | 4950000 | SL1818/850-E-TB | ||
800 | 980 | 82 | 2000000 | 4700000 | SL1818/800-E-TB | ||
750 | 920 | 78 | 1810000 | 4200000 | SL1818/750-E-TB | ||
710 | 1150 | 345 | 10800000 | 24300000 | F-800594.ZL-K-C5 | ||
710 | 1030 | 236 | 6600000 | 16600000 | Z-565686.ZL-K-C5 | ||
710 | 950 | 106 | 2230000 | 4750000 | NU19/710-TB-M1 | ||
710 | 870 | 74 | 1730000 | 3950000 | SL1818/710-E-TB | ||
670 | 1090 | 336 | 10200000 | 23100000 | F-800593.ZL-K-C5 | ||
670 | 980 | 230 | 5800000 | 15100000 | Z-565685.ZL-K-C5 | ||
670 | 900 | 103 | 2040000 | 4250000 | NU19/670-TB-M1 | ||
670 | 820 | 69 | 1450000 | 3300000 | SL1818/670-E-TB | ||
630 | 1030 | 315 | 9100000 | 20200000 | F-800592.ZL-K-C5 | ||
630 | 920 | 212 | 5200000 | 13700000 | Z-565684.ZL-K-C5 | ||
630 | 780 | 69 | 1410000 | 3150000 | SL1818/630-E-TB | ||
600 | 980 | 300 | 8200000 | 18900000 | Z-573929.ZL-K-C5 | ||
600 | 870 | 200 | 5100000 | 13500000 | Z-572367.ZL-K-C5 | ||
600 | 800 | 90 | 1960000 | 3900000 | NU19/600-E-TB-M1 | ||
600 | 730 | 60 | 1270000 | 2800000 | SL1818/600-E-TB | ||
560 | 920 | 280 | 7200000 | 15500000 | F-800485.ZL-K-C5 | ||
560 | 820 | 195 | 4400000 | 11000000 | Z-565682.ZL-K-C5 | ||
560 | 820 | 115 | 2700000 | 5100000 | NU10/560-TB-M1 | ||
560 | 750 | 85 | 1460000 | 2950000 | NU19/560-M1 | ||
560 | 680 | 56 | 1040000 | 2290000 | SL1818/560-E-TB | ||
530 | 870 | 335 | 7700000 | 16300000 | NNU41/530-M | ||
530 | 870 | 272 | 6800000 | 15600000 | Z-574099.ZL-K-C5 | ||
530 | 780 | 185 | 3950000 | 10000000 | Z-565681.ZL-K-C5 |
NEWS
所谓FAG轴承出现烧伤损伤状态是指:轴承的滚道轮、滚动体以及保持架在旋转中急剧发热直至变色、软化、熔敷和破损。造成轴承烧伤的主要原因是由于圆锥滚子轴承的润滑不良,可能使用了不正规的润滑剂,或者润滑剂过多,过少,都是不正确的。其次可能是过大载荷(预压过大)。转速过大。游隙过小。有水或其他的异物侵入。如果上面的两种情况都不是那么就是轴、轴承箱的精度不良、轴的挠度大。看到这里,我想大家都想知道解决的办法...